Company News
Shenzhen Su's heat treatment analysis on the effect of solid solution treatment on the microstructure of the specimen cooling medium

Editor:    Date:2014-09-30 17:12:59    Views:7208

Solid solution treatment with specimens of different medium cooling and then after aging treatment, the sample and then observed under the transmission electron microscope, can see all kinds of alloy sample distributed uniformly in the matrix with spherical particle zeta phase, observation can be seen in the water sample solution after aging precipitation of zeta phase number and mass more small, oil cooling sample time, air cooling and furnace cooling sample precipitation zeta phase are relatively few in number and thick. At the same time, furnace cooling specimen also found that a certain amount of zeta / beta precipitated phase. Courseware dissolution precipitation cooling speed effect of zeta phase. Because of fast cooling speed, then the quenching stress, quenching formed more wrong, for the time when the zeta phase inhomogeneous precipitation provided more nucleation sites. Moreover, due to the quenching cooling speed, so that the solid solution alloy substrate to maintain a high supersaturation, provide dynamic conditions for the zeta phase during aging precipitation. Therefore, the quenching speed is fast, the zeta phase precipitates after aging the large quantity and small dispersion. Because between the zeta phase and matrix exists potential difference, primary battery is formed in the electrolyte solution. The zeta phase of high electric potential, as the anode activation phase, the increase in the number of zeta phase, making the number of alloy Zhongyuan battery also increases, so the corrosion current increases, electrochemical corrosion resistance properties of lower alloy.

Prev: What are compared to fusion welding, brazing optimal see weaknesses? Next: Effect of Annealing on non synchronous rolling high purity aluminum foil structure
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

  • None
Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255