Bright annealed stainless steel 304

Bright annealing commonly known as bright annealing is mainly in the closed space heating makes temperature in an airtight space slow cooling after annealing at least 500 degrees to natural cooling will have glorious degree and cause no decarburization.



Order hotline: 400-6388-689

Download

  300series austeniticstainless steelheat treatment processisa typicalsolution treatment.In theheatingprocess, tocarbidedissolved in austenite, and heated to1050 ~ 1150 ℃,appropriateheatfor a short time,all dissolvedcarbidesinthe austenite,and then rapidlycooled to below350 ℃,i.e.to obtaina supersaturatedsolid solutionunidirectionaluniformaustenite.The key to thisis therapid cooling ofthe heat treatment process,the cooling raterequiredto reach55 ℃ / s,fastafter solutionbyre-precipitation ofcarbidestemperature zone(550 ~ 850 ℃).Holding timeto beas short as possible, otherwise thecoarse grains, the impact ofsurface finish.


Su's heat treatment Co. Ltd. was founded in 1990, after decades of development, scale is continually expanding, is located in Shajing Town Baoan District Shenzhen City Bridge second industrial zone, covering an area of 3000 square meters, the main business is to take all the metal, alloy steel, beryllium copper, heat treatment of high speed steel, cryogenic treatment (-196 C), nitrogen gas, liquid nitrogen, QPQ salt bath production line, high-frequency quenching, blackening and carburizing, the surface of hard and stainless steel processing.
The company is equipped with power of heat treatment technology, established a perfect quality testing equipment, equipped with vacuum quenching furnace, vacuum furnace, pit furnace, furnace, liquid nitrogen atmosphere furnace, rotary furnace, large mesh belt furnace, improve metallographic inspection equipment, material failure analysis, scientific management and complete, rigorous technology, skilled operation.
Company will be excellent quality and perfect service, and actively challenge, satisfy customer demand, has passed ISO9001:2000 in 2003 September (SGS) international quality certification. Has now become a reputable manufacturers.


Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:
Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255