Pre-hardened mold material

Editor:    Date:2014-05-05 13:56:23    Views:9318

Since the 70 s, the world has put forward the idea of pre hardened, but because of machine tools and cutting tools, stiffness of the pre hardened hardness can not meet the use of mold hardness, so in the process of the hardening technology r&d. Along with the improvement of the performance of the machine tools and cutting tools, mold material hardening technology development speed, to the 80 s, the international industrial developed countries in plastic mould materials using the proportion of the pre hardened module has reached to 30% (currently at more than 60%).

Our country in the mold material hardening technology, late start, small size, it is can not meet the requirements of domestic mold manufacturing. Using pre hardened mould material, mould manufacturing process can be simplified, shorten the mould manufacturing cycle, improve the manufacturing precision of the mould. Predictably, with the development of processing technology, the pre hardened mould materials will be used for more mould.

Prev: Mold surface treatment technology Next: None
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance corrosion and wear resistance
Austenitic stainless steel under different heat treatment techniques for the performance of the different resistance to corrosion and wear properties of a great relationship: the number and morphology of precipitates in the pure wear conditions, no corrosion, material quality loss is influenced by mechanical factors.
Vacuum heat treatment of the problem
Vacuum heat treatment processing, the processing surface of the product is often a problem, "colored" areas appear. Obtain appearance of bright, no coloring effect is the common goal of product processing vacuum furnace manufacturers and users to pursue research and development.
Vacuum heat treatment technology to resolve
Comprehensive technology of vacuum heat treatment vacuum technology and heat treatment technology of two professional combination, refers to the heat treatment process of all or part of the vacuum condition. Is generally believed that the vacuum furnace is divided into high, high, medium and low vacuum.
Factors that affect the performance of the heat treatment
Today su shi heat treatment come to you of what the factors in the use of vacuum heat treatment furnace heat treatment will affect the performance of the heat treatment:

1
Brazing of aluminum frame
Product:Brazing of aluminum frame
2Cold die steel heat treatment technology
3High-frequency quenching
4Stainless solution treatment
5SUS420 blade heat treatment
6Vacuum hardening

Similar Articles

Latest News

History

Set Home Page  |Contact|News|Set Map

Su's heat treatment (Shenzhen) Co., Ltd.  Guangdong ICP No. 14020634
service hotline: 0755-27291255
Fax: support for 0755-27293730
E-MAIL:sushirechuli@163.com
Company address: Shenzhen, Baisha bridge Second Industrial Zone No. 14

(Workdays:9:30-18:00)

Online QQ



Service Hotline

0755-27291255